Wednesday, January 14, 2015

[MW:22725] Ring Type Joint Gasket Hardness Test

Hellow


As per ASME B16.20, for ring gasket material, Soft iron gasket as well as other materials are mentioned, see below table from ASME B16.20

 

there are some parameters should be specified for testing soft iron and stainless steel in a symbol as below:

 HBW Ball diameter/F/Dwell time


 considering Ring Type Joint Thickness the ball diameter should be 10mm since the ball diameter should be as large as possible. is this correct?


Normal dwell time is between 10 to 15 sec and it seems to be a good choice for R.T.J hardness testing.


but my major question is about "F" parameter which should be specified in relation with D, F/d and material.

in order to that please inform me what is the best choice for "F" to test HARDNESS of soft iron(D) and stainless steel(ss) R.T.J ?


HBW 10/3000/15 LOOKS TO BE GREAT FOR SS???

 what about SOFT IRON MATERIAL?

 LET ME KNOW about that...





Best Regards

Miad Bahrami

Behta Industrial Gasket Co.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKUA0MmNLB94S%3D%3DTwK2iHx-3XzEX%2BAgFi6C%3DVeQ%2B%3Dg02ydkJwQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...