Wednesday, January 14, 2015

[MW:22723] Impact test requirement for P.No.1.

Dear All,


Please provide ASME sec IX interpretation/clause to solve the below issue.

Backgorund:

Base metal-1 thk : 40 mm (IS 2062 Gr.B)
Base metal -2 Thk : 3 mm (IS 2062 Gr.A)

Filler wire : ER70S-6 (1.2 mm)
Gas : Co2.

Question : Base metal and deposited weld metal thickness range for the above combinations (Impact test is required) ?.






--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ%2Btj09ks%3DHmmOVu%2BujhoTJ7vPJm2yMSraevZdmcwCupTRP27A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...