Use ER 316L.
Regards
Prem Nautiyal
9769316004
On Tuesday, August 12, 2014 1:56 PM, S.Mohammed <mohd52100@gmail.com> wrote:
Dear all,
What should be the best filler wire for 304L to 316L welding.
Service temp : below 150 & above 400.
Regards
Mohd.
-- Mohd.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments