Monday, June 2, 2014

[MW:20954] branch connection to pipe -fillet size calculation

Dear all
          For full penetration  branch welding , a groove and Fillet is welded . The groove is completely filled up.

          At the  longitudinal axis of the main pipe, the fillet is welded as 15 mm as per drawing.

Question - What shall be the fillet on the  radial zone of the pipe?
 Refer figure attached.The fillet area at  "B"  is of discussion interest.

Pl. inform any back up /technical document  for required fillet guidelines

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone