Re: [MW:20492] RE: 20443] Weld joint Repair

Dear,

 

Regards to your query, It is not advisable to repair the weld joint more than twice, as it could impact the micro structure of the HAZ and the base metal. The standard has not put any restrictions on the number of times can a joint be repaired, but usually clients doesn't allow more then two times. It is up to the client discretion and project specification, but no reference you find the code. The code says the joint shall be repaired by using the qualified procedure/ same procedure and tested by the same method as used initially for the joint.

 

Thanks

M. Javeed

Quality Supervisor- Welding. 



On Tue, Apr 1, 2014 at 3:45 PM, Faisal Shahzad Meer <fmeer@gccksa.com> wrote:

Dear

 

Regarding Pipeline as per Saudi Aramco standard Two time repair is allowed even for grade 70 materials ,third time we have to go for CUT out. I think there is nothing specific in the code regarding attempts of repair only customer specification may dictate this issue.

 

Regards

 

Faisal Shahzad Meer

Project Quality Supervisor-Welding

J-505, Saudi Aramco Wasit Downstream Pipelines Project

 

TEL :+966 3 6795805-7 Ext. 124|www.gccksa.com

E-mail  fmeer@gccksa.com 

+966 - 553919249

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saidur Rahman
Sent: Monday, March 31, 2014 9:42 PM
To: materials-welding@googlegroups.com
Subject: [MW:20443] Weld joint Repair

 

Dear Experts,

I am working on 30" High pressure gas transmission pipeline project. Today i found that in one RT film there was 100 mm Internal undercut. After repair RT film shows that again 45 mm internal undercut with Internal Concavity. But my superior says that only one time repair is acceptable & joint should go for cut-out  because if again repair then Susceptible micro structure will form. my question is How many times repair is acceptable? Pipe material API 5L-X 60. thickness= 14.3 mm

and also for Process piping how many times repair is acceptable if PWHT is a service requirement?

Regards,

Md. Saidur Rahman

QA/QC

GTCL

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...