Client want to establish WPS by combining the below both PQRs of Section IX to get additional advantages. Please review and tell, whether this is possible and if not why? if yes give details.
Vessel MDMT: -47.5
WPS # 38 is made by combining two PQRs:
PQR 1: SMAW :::::: 5.98 mm thk coupon
Material: SA 516 Gr 60 to SA 516 Gr 70.
Thickness range: 2.99 to 11.96 mm
Test temp: -59 deg C.
PQR 2: SMAW ::::::: 10 mm thk coupon
Material: SA 516 Gr 60 to SA 516 Gr 70.
Thickness range: 10 to 20 mm.
Test temp: -51 deg C.
Thanks in advance
Regards
Santosh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment