Dear Friend,
Please read carefully part QW.191 and specially QW 191.1.2, then you will find your answer for all indications. Following to that you can find acceptance criteria for UT.

Regards


On Mon, Nov 25, 2013 at 10:51 AM, Kumar <sk7920541@gmail.com> wrote:
Dear All,

When conducting  WPQT(welder performance qualification test), the
acceptance criteria for both visual & RT is SEC.IX, but the these are
seemed to be much short & liberal. like,

Visual- complete fusion & penetration only required for visual, then
what about undercuts, underfill, re-inforcement height etc ?
RT- only chart given is for porosity comparison (attached herewith).
what about slags and other defects?

If anybody has more details of the above part of  SEC.IX, please share.
due to these reasons some times we find difficulty to judge sub-con
welder performances.
could we refert the construction code of the intended project in that case?
Appreciating your valuable feedbacks.
Thanks in advance,
Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...