Based on the image ,the stain might caused by the corrosive  fluid   used in the vessel and the leakage  near the heat affected zone.you may  find out the nature of fluid by  microbiological test then make a decision.
Regards,
S.ANANDH
QA/QC INSPECTOR 
NSH CORPORATION
SADARA CHLORINE&BRINE PROJECT.
SAUDI ARABIA.
  On Wednesday, 20 November 2013 4:22 AM, kalidindi raju <eswar.iitb@gmail.com> wrote:
  
  Dear Friends,
On a recent inspection of a Stainless Steel Vessel, there were some corrosive stains observed on near the weld.
Please refer to the pictures attached.
  The stains indicate a leakage/flow behavior of the containment.
However, when observed visually there was no leakage of any liquid.
The vessel was in service since 2008.
Material of construction is Stainless Steel SS 316.
  What could be the probable cause of this behavior?
Please share your views.
Regards,
Eswar Raju.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments