If you weld small diameter and less thickness, TIG welding may be preferred.
 
Thanks & Regards


J.Gerald Jayakumar
00974-55835810


On Thursday, November 21, 2013 1:28 PM, Prabir Kumar Singh <prabirkumarsingh86@gmail.com> wrote:
Dear All

In socket welding of high pressure steam pipeline we have to weld by
SMAW . But our Client ask us, first pass of welding should be by  TIG
welding. Then SMAW welding. Is TIG welding necessary in socket
welding. Please suggest with any code reference

With Regards:
Prabir Kumar Singh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...