Dear All,
When conducting WPQT(welder performance qualification test), the
acceptance criteria for both visual & RT is SEC.IX, but the these are
seemed to be much short & liberal. like,
Visual- complete fusion & penetration only required for visual, then
what about undercuts, underfill, re-inforcement height etc ?
RT- only chart given is for porosity comparison (attached herewith).
what about slags and other defects?
If anybody has more details of the above part of SEC.IX, please share.
due to these reasons some times we find difficulty to judge sub-con
welder performances.
could we refert the construction code of the intended project in that case?
Appreciating your valuable feedbacks.
Thanks in advance,
Kumar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-