Re: [MW:18538] Current & Voltage Ranges for WPS

Hi Kishore,

you can get those recommended datas from manufacturers Catalogues , like ESAB, Hyundai, Lincoln, Thyssen,  whatever brand you have selected.

for each size and the position of welding .

Before making PQR, you should always refer to the welding manufacturer's recommendation for Amps, Volts, polarity, type of coating, AWS Classes etc .

Cheers ,
Saravanan ,
Korea




On Thu, Aug 29, 2013 at 2:07 PM, Thota Kishore <krish.royal18@gmail.com> wrote:
Dear Sir's,

Good Morning.!


I have to prepare WPS&PQR for E6013 and E7018 in 2G/3G(up hill)
position. So I wish to know the range of current and voltage for
procedure specification/qualification. Is there any standard
table/chart for current/voltage reference or its a practice.

Kindly suggest me.

--
 Thanks & Regards,

T KISHORE
+91 9951141681

[image: Description: Description: Description: Description: Description:
cid:000801cb3f83$888f00d0$2d01a8c0@Accounts2]


*P**     **I Pledge to take personal action to help solve the climate
crisis by reducing my own CO2 pollution as much as I can offsetting the
rest to become "Carbon Neutral". *
*
*
*Spread environmental awareness to avoid Global Warming. *
* *
*Save Nature... Save Future...*

**

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...