Re: [MW:18512] PWHT of SA 612N used in cryogenic service

SA 612 falls under P number# 10C, for the mentioned thickness PWHT is not required (refer Table UCS 56)


On 25 August 2013 19:58, <dstevenson@cvatanks.com> wrote:
We are currently manufacturing tanks for CO2 transport service using Sec VIII Div. 1 ASME and I am being told the tanks do not require PWHT? The tanks are shell 7/8 inch Heads are 7/16 the process is subarc.
Can anyone point me to a section or code that would explain why we would PWHT or where we would not have to PWHT these units?
Thank you for aquick reply

-

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...