Re: [MW:18508] Ferrite Content Check on root or final weld

Sandvik 25.22.2LMn would help you in achieving the required FN 2.
Tested.
Additionally, you may use WRC1992 diagram to predict ferrite using different welding consumable.

Octane


On Sat, Aug 24, 2013 at 4:01 PM, Rudolf <rudolf_jude@yahoo.com> wrote:
Hi in my opinion it should be specified in the contract spec if they want specifically for every  weld process. However the probe has to be in contact with the weld metal to get the FNo and if there is no sufficient opening for the probe to fit in then it would be difficult unless you access from the back side of the weld. 

The range stated by you is a bit tight normally it is from 3 to 8, and I did this tests recently and it was around 5+. 

This is just my experience.
Keep posting the results. 

Regards

Sent from my iPhone

On 24 Aug, 2013, at 8:30 PM, "Ankit PAtel" <ankit.patel@orientalindia.net> wrote:

Dear Exerts,

 

Kindly suggest on following issue

We have a job on which ferrite content test is essential. we are welding with root run by GTAW & sub sequent layer by SMAW. Please confirm whether it is essential to check the ferrite content of the root or final weld.(top of the weld.)

Base Material-SA 240 TP 316L

Filler Wire/Electrode:- ER-316L & E-316L

Also our requirement is 2FN to 5FN kindly suggest any filler wire/Electrode manufacturer.

 

Regards

 

<image001.jpg>

Ankit Patel
Engineer Quality

Oriental Manufacturers Private Limited
A: P.C.C. Notified Area, Ranoli Station Road,

 Ranoli -391 350 Baroda Gujarat India

T: +91.265.223 1663/2232936

F: +91.265.223 0171
E:  ankit.patel@orientalindia.net 
W: http://www.orientalmanufacturers.com

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...