Dear Ramin,
You will achieve same properties in both base metals (just for weld metal). For example impact specimen with notch exactly in the center of weld metal, the same properties will be seen. Same subject for All-weld metal tensile test specimen.

However above notes will be tend to truth, whenever the weld metal will be more and more (I mean cross section of deposited weld metal).

Regards


On Wed, Aug 21, 2013 at 12:20 PM, Ramin <ramin.ab82@gmail.com> wrote:
Dear experts,

Please advise me;
there are 2 different steel plate with the exact same chemistry. One of them is traditional rolled steel around 1200 degree Celsius with coarse grain structure and one another is thermomechanical rolled in 750 degree Celsius very fine grain structure.
I don't want to weld them together, actually I'm wondering if we use same consumables for welding of each plate separately, how is the mechanical properties (charpy and tensile) of weld metal for these different structure? And why? Does thermomechanical steel provide better quality ?
Same welding process: SAW
Same heat input, wire, flux, dilution, size, ...

Regards,
Ramin

Sent from my iPhone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer

Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...