Re: [MW:18476] Clarification on Sec. IX interpretation: IX-92-87

PQR qualified on 1" thickness (with notch toughness) qualifies for minimum thickness of 5/8" as per QW-403.6. Maximum remains at 2"

Octane


On Mon, Aug 19, 2013 at 1:38 PM, Harikrishnan N S <hari.qaqc@gmail.com> wrote:

Interpretation: IX-92-87

Subject: QW-403.6, Base Metals; and QW-409.1, Electrical Characteristics

Date Issued: February 14, 1994

File No: 93-151

 

Background: Two PQRs have been qualified to support a WPS with notch toughness requirements and having a qualified base metal thickness range from 5/16 in. to 2 in. inclusive. One PQR was qualified on 1 in. thick material with a maximum heat input of 85,000 J/in. The second was qualified on 5/16 in. thick material with a maximum heat input of 45,000 J/in. All other essential and supplementary essential variables are the same.

 

Question (2): Is the heat input value of 85,000 J/in. applicable to base metal thicknesses between 5/8 in. to 2 in. and the heat input value of 45,000 J/in. applicable to base metal thicknesses between 5/16 in. and 5/8 in.?

 

Reply (2): Yes.

My Query:

1)    1)  Why they are limiting heat input based on material thickness as material thickness is not involved in heat input calculation? Is this related to cooling rate?

2)     2) For PQR done on 1in. thk. with max heat input of 85,000 J/in. How they calculated the minimum qualified thk. as 5/8 in. (isn't it 1 in. to 2 in.?)

Re





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...