Hi Siva,
Please review the attached PDSs MIG & TIG Brazing filler alloys . As you need assistance for your project work hence this mail. For more details on dissimilar brazing you may visit Fontargen web-site thru the link below my signature. We can discuss more on our products out of forumās domain .
Hope this helps..
Thanks
With Kind Regards
Amitabha Bhattacharya
Head-Application Technology
Bohler Welding Group India Pvt. Ltd.
A-140, Road No 23, Wagle Industrial Estate
Metropolitan, Ground Floor
Thane 400 604, India
Ph: +91 22 2582 8855/4228 4400
Mobile ;+91 9833998246
Email: amitabha.bhattacharya@bwgindia.com
Web: www.bohlerweldinggroupindia.com
A Bƶhler Welding Group Company
This email message and any attachments are for the sole use of the intended recipient(s) and contain confidential and/or privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message and any attachments
From: Siva Chidambaram <mechsivachidambaram@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 15 August 2013 3:07 PM
Subject: [MW:18437] Bronze to carbon steel welding.
Hi Friends,
In my project, there is welding between bronze and carbon steel. Can anyone kindly say me what electrode to be used for welding.
M. Sivachidambaram
+971561530899
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments