Re: [MW:18466] Re: heat input calculation in welding

calculate for individual pass and while writing wps, mention the maximum heat in put among passes


On Sun, Aug 18, 2013 at 1:54 AM, <kzarrinnaghsh@gmail.com> wrote:
Hi there, heat input limitations are applicable to each weld pass and do not apply cumulatively.
-----Original Message-----
From: Scott Loew
Sent:  17/08/2013, 21:16
To: materials-welding@googlegroups.com
Subject: [MW:18459] Re: heat input calculation in welding


take a look at this Video
http://vube.com/Data+Scope+Solutions

On Thursday, January 27, 2011 10:19:23 PM UTC-6, sandy wrote:
>
> Hi everybody
>
> I have one query regarding the heat input.
> If I am welding a joint with multipass, then I have diffrent heat
> input for every pass depening on the parameters. now I want to know
> which heat input shall be taken into consideration for the effect of
> heat input on base metal, cauz every pass has its effect on base metal
> and after every pass due to the previous heat input I am giving extra
> heat in the base metal.
> So I want to know should I take individual heat input or sum of all
> heat input for getting the exact effect of Heat input on base metal.
>
> Regards
> Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...