Re: [MW:18458] Re: May E8018-C1 substitue E8018-G to weld Corten Steel

E8018-G is general low alloy steel electrode means no fixed chemical composition requirements for all the alloying elements until or unless agreed between the supplier and purchaser. You should not be using this in place of E8018-C1 or E8018-W2.
Like E8018-C1 requires at least 2% Ni versus only 0.5% min. specified in E8018-G.

(attached find the chemical requirements of E8018-C1 and E8018-W2)

Octane


On Sat, Aug 17, 2013 at 3:34 PM, Abuzar Malik <abuzarmalik@gmail.com> wrote:
Hi everyone. i am also facing the almost same issue. we are short for E 8018 W2 electrode for corten steel. now contractor wanted to use  E 8018 G electrode as a W2 replacement. kindly guide me whether to allow him or not? reply kindly?

On Thursday, 20 October 2011 14:16:58 UTC+5, Tunisian Quality Engineer wrote:

Hi all

For welding Corten steel, we have in storage E8018-C1 Electrod, may it substitue  E8018-G, how can confirm ?

Regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...