Saturday, August 31, 2013

[MW:18547] Re: How to select the IQI wire

Dear All,

Let me know what is the difference between ASTM, FE EN & DIN wire. What material is suitable for which wire?

Regards,
Raheel Arif

   

On Monday, August 2, 2010 8:48:53 AM UTC+4, venkat ramana wrote:
Dear All,
 
let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.
 
Thanks & Regards
venkat (QC)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...