Dear All,

        Reference standard mentioned for NACE service valves is MR0175/ISO15156.As per this standard test certificate(lab report) must declare PREN no.mentioned in Table D.1.
       Our  valves are made of carbon steel body bonnet,13%Cr Trims & SS316+Graphite filler gasket.In ITP & specification gasket's chemical analysis report is required.
      Is it necessary to declare PREN no. in gasket's chemical analysis report as it is SS316?

         Thanks & regards.

Swapnil D'Britto

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...