I have one query regarding the heat input.
If I am welding a joint with multipass, then I have diffrent heat
input for every pass depening on the parameters. now I want to know
which heat input shall be taken into consideration for the effect of
heat input on base metal, cauz every pass has its effect on base metal
and after every pass due to the previous heat input I am giving extra
heat in the base metal.
So I want to know should I take individual heat input or sum of all
heat input for getting the exact effect of Heat input on base metal.

Regards
Sandeep Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...