Re: [MW:17826] 9.3.8 Slag Inclusions API 1104 RT

Dear sir.

According to your example given below,
When we consider the width of the indication, then you have to reject since it exceeds 1.6mm.and I believe you no need to worry about length.

Thanks n regards
Raj

Sent from Yahoo! Mail on Android



From: Ghaith NDE <ghaithnde@yahoo.com>;
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>;
Subject: [MW:17818] 9.3.8 Slag Inclusions API 1104 RT
Sent: Mon, May 27, 2013 5:48:32 PM

Dears experts\
there is acceptance  for ISI & ESI  RT  1104  my question  is  in case one of these conditions is found  for example
when i  have done interpretation I found indication ESI has width   2mm  and length 9mm  this indication rejected because it exceed 1.6mm   or not because  it should be has length more then 2" to rejected .  
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...