Dear
I find your main concerns as if the inspector does not know his job.You also says that your management has taken this issue very seriously.I believe they should taken it during welder qualification.
I believe your client inspector may be having enough experience where he clearly states the repair.
Please note that where limited information available for the imperfection by any method you as a constructor demonstrate any other method to prove that internal protrusion/penetration is with in the code limit. Destructive or NDT for one or two dispute cases.
The case of intelligent pigging will come later if it required as per specification. Excess penetration will stuck the pig in the line.
Please read below clauses of API-1104. specially rights of rejection.
13.8.4 Rejection Based On Reinforcement
The inside-diameter weld reinforcement shall not be raised
above the parent material by more than 1/16 in. (2 mm). The
outside-diameter weld reinforcement shall not be raised
above the parent material by more than 1/8 in. (3 mm).
13.
9.2 RIGHTS OF REJECTION
All nondestructive test methods are limited in the information
that can be derived from the indications they produce.
The company may therefore reject any weld that appears to
meet these acceptance standards if, in its opinion, the depth of
an imperfection may be detrimental to the weld.
On 27 May 2013 12:24, Dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
Dear friend ,that code is API 1104..my question is excess penetration how is measuring the rt film like ruler scale..your knowledge it is possibleThanksDominic V.K.
On Mon, May 27, 2013 at 10:28 AM, Babur Khan <mbabur.bwp@gmail.com> wrote:so and same like API 1104 have criteriaas per thisDear friend,1st you mention construction code which applicable if ASME B31.3-2008 then see Table 341.3.2 Acceptance Criteria for Welds and Examination Methods for Evaluating Weld Imperfections
L Height of reinforcement or internal protrusion [Note (8)] in For T w, mm (in.) Height, mm (in.)
any plane through the weld shall be within limits of
the applicable height value in the tabulation at right, ⤠6 (1ā4) ⤠1.5 (1ā16)
except as provided in Note (9). Weld metal shall merge > 6 (1ā4), ⤠13 (1ā2) ⤠3 (1ā8)
smoothly into the component surfaces. > 13 (1ā2), ⤠25 (1) ⤠4 (5ā32)
> 25 (1) ⤠5 (3ā16)
M Height of reinforcement or internal protrusion [Note (8)] Limit is twice the value applicable for L above
as described in L. Note (9) does not apply.
--On Mon, May 27, 2013 at 9:28 AM, Dominic v.k.dominic <v.k.dominic@gmail.com> wrote:
--Dear Expertise,I have this issue please anyone clarify me,One QA/QC- Inspector 20 years Experience person he rejected one 24" pipe line RT film because of excessive penetration by measuring the dimension with a ruler and required the joint to be repaired..This is Acceptable or Not Acceptable.if Acceptable where is mentioned the code?Please clarify me, Because my management take this issue very seriousBest RegardsDominic V.K.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--Regards
BABUR KHAN LASHARI
Welding Inspector
(QA/QC)
SATORP (JERP)
Mob: +966 (0) 56 2179280
Skype Id : babur.lashari
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments