Re: [MW:17813] Using of electrodes (2.5mm) one brand upto certain thickness and using 3.2 mm electrodes of other brand in remaining thickness.

if mechanical property is same ,u can use bcoz according to sec 9 dia is not essential variable for welding so according to me u can use it,unfortunatly the same issue is on my site but our client agree to use different comany of electrode but both the company had pass their electrode qualification test.

On Mon, May 27, 2013 at 7:53 AM, Talluri Venkataramana <venkataramana.talluri12@gmail.com> wrote:
Dear experts

Kindly guide me Using of electrodes (2.5mm) one brand upto certain thickness and using 3.2 mm electrodes of other brand in remaining thickness. Our scope is welding of 12mm thick Pipe in offshore platform. we have 3.2mm electrodes of Manitowoc and 2.5mm electrodes of ESAB. Specification of electrode is AWS A5.5, E9018M-H4. 

As per my opinion with the same mechanical properties can be used. Guide me if any thing is different.

--
Best Regards
T.V.Ramana

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
----------------------------
QA/QC Inspector
Samsung Engineering Co.Ltd.West Qurna Field Phase#2 PRJ(IRAQ)
Hello:+964-7802509282
Mail @ aslab786@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...