Re: [MW:17796] Polarity difference in WPS

Agree with Vijay you can revise the WPS with -ve polarity without the need for requlification .
 
Very Best Regards
Behrooz Alavi

From: Malusare Vijay <vijaymalusare07@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, May 25, 2013 2:15 PM
Subject: Re: [MW:17794] Polarity difference in WPS

Yes You Can Revised without re -qualification.


Regards,
Vijay Malusare


On Sat, May 25, 2013 at 4:31 PM, Lalu r p <lalucpt@gmail.com> wrote:
Dear Experts

In my company we have a wps qualified in last year with AWS D1.1 for structural steel welds.But now the client has raised a problem that in that wps the polarity of the electrodes which is used for the root run is wrong.The electrode used was E-7016-1 and as per standard the polarity should be +ve. But in place of that we used -ve polarity and the PQR is qualified with that.Since I am new to this company I have to solve the issue for submitting the final dossier.So my question is that whether  this WPS can be revised without re-qualification.

Thanks & Regards 

LALU R.P
QA/QC ENGINEER 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...