for wps no problem, but for welder u have to qualify in 2G position

Pandithan
welding Consultant


On Fri, May 24, 2013 at 11:33 AM, Himayat Ali <ali.himayat@gmail.com> wrote:
Dear member, 

A fabricator who does production welding in a particular orientation may make the tests for procedure qualification in this particular orientation. Such qualifications
are valid only for the positions actually tested, except that an angular deviation of ±15 deg is permitted in the inclination of the weld axis and the rotation of the weld face as defined in figure QW-461.1.

On Thursday, May 23, 2013 1:35:47 PM UTC+3, KABEER wrote:
Dear experts,

IN OUR COMPANY SS WELDING WORK UNDERGONE .SHEET THICK 3.15MM. PROCESS TIG WELDING. TWO NOS OF SHEETS WELDED TOGETHER AT THICKNESS AREA UPTO 25MM LENGTH.WPS AND WELDER QUALIFICATION AVAILABLE FOR 1G ONLY.BUT WELDER HAS DONE WELDING AT 2G POSITION. AS PER ASME SEC IX QW 405 POSITION GIVEN IN NON ESSENSIAL VARIABLE.MY DOUBT IS WELDER HAS TO QUALIFY 2G POSITION OR 1G ENOUGH.KINDLY CLARIFY AS EARLY AS POSSIBLE

THANKS AND REGARDS

S.M.KABEER AHAMED

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...