No, it is not required.    See QW-200.2 (b) – Contents of the PQR.  “The completed PQR shall document all essential and , when required supplementary essential variables of QW-250 through QW-280 for each welding process used during welding of the test coupon.  Non-essential and other variables used during the welding of the test coupon may be recorded at the manufacturers or contractors option.  . . . “  There is no requirement for recording a WPS number.

 

Further, regarding the form provided by Sc IX “ Form QW-483, see Nonmandatory Appendix B, has been provided as a guide for the PQR.  . . .”

 

See also the last paragraph of QW-100.1 “The PQR documents what occurred during welding the test coupon and results of testing of the coupon.  As a minimum, the PQR shall document the essential variables and other specific information identified in Article II for each process used during welding the test coupon and the results of the required testing.  In addition when notch toughness testing is required for procedure qualification, the applicable supplementary essential variables for each process shall be recorded.”

 

For ASME Section IX it is NOT required.   

 

When stating requirements, one should provide Code reference(s) otherwise indicate it is an “opinion”.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of james gerald
Sent: Thursday, May 23, 2013 2:15 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17760] WPS no. on PQR

 

Yes it is required.

 

 

 

Thanks & Regards

J.Gerald Jayakumar
00968-99438165

From: kannayeram gnanapandithan <kgpandithan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, May 23, 2013 8:43 AM
Subject: [MW:17758] WPS no. on PQR


Is it required to put WPS no. in PQR, if so pl give code ref
Pandithan
Welding Consultant

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...