Friday, May 31, 2013

[MW:17843] Regarding baking of low hydrogen electrodes

Dear experts,

                        I have query regarding baking of low hydrogen electrode, is there any universal rule/standard governing these as in some project rebaking is not allowed whereas in some project re-baking can be done only 1 or 2 times.


Query1: how many time can we bake the low hydrogen electrodes, if over baked what will be the consequence.

 

Query2: after baking we transferred to holding oven maintain at 150 ° C,  how long we will keep electrodes at these temperature


Regards

shashi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...