Dear Sajid,
 
One of the options available to you is to get the WPS qualified and welder qualification as per WPS, if both are satisfactory then you can assume all the welds are fine otherwise you will have to decide b/w cutt off and ignore keeping into view ur application criticality.
 
Ammar Shaikh

On Wed, Jan 16, 2013 at 12:44 PM, joseph mbé <mbejoseph@yahoo.fr> wrote:
You should make that welders are qualified before the start of the job! that's just not professionnal. now, i think you should perform the test (RT) on as welded joints to prove their quality instead of qualifing welders after work completion.

rgds

 
Joseph Faustin Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
 


De : sajeed zaheer <sajeed7674@gmail.com>
À : materials-welding@googlegroups.com
Envoyé le : Mercredi 16 janvier 2013 7h12
Objet : [MW:16518] Fwd: welder qulification test or performance


Dear experts,
 
for structural project the sub vendor has done welding with out qulified welders now this sub vendor is saying they will produce wqt with in one week with previous date.so my question is wheather it is accptable ,if it is acceptable please provide the refrence. awating for your reply.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...