Is it galvanized pipe are P1 group material?. E309 are dissimilar electrode between carbon steel joint to stainless steel.
Sent from my iPhone
On 16/01/2013, at 2:06 PTG, G Sreenivas Rao <gsrinivasg3@gmail.com> wrote:
> dear mohd
> we can do the welding GI to SS, provided the GI coating on pipe weld
> are to removed by grinding and welding can be carried out with E309
> welding electrode.
>
> regards
> GSR
>
> On Wed, Jan 16, 2013 at 7:52 AM, <mohdfirdaus.abdrahim77@gmail.com> wrote:
>> Dear Expert,
>>
>> Kindly need your information for stainless pipe weld to G.I pipe. Is it possible to do?. If yes, shall follow which material grouping for G.I pipe?. I need to prepare the WPS for this dissimilar welding. I need to know filler metal to be used etc;.. I hope all of you can guide me. Thank you.
>>
>> Mohd Firdaus Abd Rahim
>> QA/QC
>>
>> Sent from my iPhone
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment