Re: [MW:16475] Clarification on ISO 15614-1

Dear RH,
 
Fillet Weld test is required , if u r qualifying for Fillet weld,,,(if & if u qualify Butt weld -partial & full penatration,etc........) ...
 
With Regards,
Ashish Pathrabe


 
On Tue, Jan 8, 2013 at 10:33 AM, Rohit mn <rhmalhotra84@gmail.com> wrote:
Dear All,
Kindly Clarify below highlighted in red fonts...what should we understand by predominant weld and how to select????....as I understand all weld carry load.
 
ISO 15614-1
8.4.3 Type of joint/weld

The range of qualification for the type of welded joints is as used in the welding procedure test subject to limitations

given in other clauses (eg diameter, thickness) and additionally:

a) Butt welds qualify full and partial penetration butt welds and fillet welds. Fillet weld tests shall be required

where this is the predominant form of production welding.


rgds
--
Rh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...