Hai,
Mostly project specs. spells hardness requirements.
the attached file might be useful to you.
regards
R Vairamuthu
Subject: [MW:16411] HardnessP-91 Material
Date: Wed, 2 Jan 2013 09:36:41 -0800
From: ARudder@IrwinIndustries.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Mostly project specs. spells hardness requirements.
the attached file might be useful to you.
regards
R Vairamuthu
Subject: [MW:16411] HardnessP-91 Material
Date: Wed, 2 Jan 2013 09:36:41 -0800
From: ARudder@IrwinIndustries.com
To: materials-welding@googlegroups.com
Sir,
What's the Max hardness for weld metal and HAZ for P-91 Material per B31.1
Thank You,
Tony
QA.Manager.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment