Dear All,
Kindly Clarify below highlighted in red fonts...what should we understand by predominant weld and how to select????....as I understand all weld carry load.
ISO 15614-1
8.4.3 Type of joint/weld
The range of qualification for the type of welded joints is as used in the welding procedure test subject to limitations
given in other clauses (eg diameter, thickness) and additionally:
a) Butt welds qualify full and partial penetration butt welds and fillet welds. Fillet weld tests shall be required
where this is the predominant form of production welding.
rgds
--
Rh --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment