Please find the details below tagged
1. Construction code to be followed.-ASME B31.3
2. Requirement of impact test (temperature and energy).-NO IMPACT TEST REQUIRED.
3. Grade of API 5L pipes to be welded.-API5L PSL2.
4. Whether WPS/PQR for SA 106 Gr.B(P1-P1) Impact tested. If tested -Test temperature.-NO
WPS/PQR NOT IMPACT TESTED SINCE THE JOB being fire water line pipe DOES NOT REQUIRE IMPACT
TEST.
5. Electrode/filler material used in the WPS/PQR.-ER70S-6
Expecting your kind reply.
krishna
Catch India as it happens with the Rediff News App. To download it for FREE, click here
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment