Re: [MW:16123] Methods & procedure to accept that joint without hydro test again

Dear Sir,

In process inspection can be done for that joint as per ASME B 31.3.

Radiographic testing of that joint can be done in consultation with client/owner and review can be done as Golden Joint/ Tie in joint (stringent inspection criteria in discussion with client to be followed).

Regards,
Hareesh K v
+91-8306703707


On Sun, Dec 2, 2012 at 8:40 AM, PK M <pkmqaqc@gmail.com> wrote:
Dear Experts,

A certain joint cut & re weld in spool which hydro test completed, is there any methods & procedure to accept that joint without hydro test again?


Thanks,

Pkm.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...