Monday, December 3, 2012

Re: [MW:16115] I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?

Hi!
 
No , It is not good engg practice . The preheating is prefered to be carried by  LPG or equivalent  flame and not byOxy acetylene flame (As there is a tendancy of burning of steel due to high temp)
 
Regards
 
Hegde P.B.

--- On Sun, 2/12/12, PK M <pkmqaqc@gmail.com> wrote:

From: PK M <pkmqaqc@gmail.com>
Subject: [MW:16100] I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?
To: materials-welding@googlegroups.com
Date: Sunday, 2 December, 2012, 10:03 PM

Dear Experts,

I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?

Thanks,

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone