Monday, December 3, 2012

[MW:16114] RE: 16100] I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?

Not accepted, cutting torch is using mixture of oxy-acetylene which can cause oxidation in that area.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PK M
Sent: Sunday, December 02, 2012 8:34 PM
To: materials-welding@googlegroups.com
Subject: [MW:16100] I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?

 

Dear Experts,

 

I did preheat in carbon steel by cutting torch instead heating torch. Is it acceptable or not, if not means why?

Thanks,

Pkm..

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...