[MW:16098] Re: Welding CS to SS ? THICKNESS > 19 mm

not required if the code is asking then you have do it
On Wednesday, 14 November 2012 13:09:44 UTC+5:30, Tunisian Quality Engineer wrote:
Dear experts,

  We have one doubt. Need your help.

We have to weld carbon steel (A106-C)  to austinitioc stainless steel (316 L  grade), thickness > 19 mm.

PWHT in this case is mandatory ? if yes, they're   some restrictions ?


Regards.

--
زكرياء غراب
GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone