Re: [MW:14147] alignment tolerance

Dear Prashant

It is depend on thickness, for more details please see UW-33

Regards
Mahesh


From: prashant pansare <prashantpan_99@yahoo.co.in>
To: mat wel <materials-welding@googlegroups.com>
Sent: Tuesday, April 24, 2012 7:58 PM
Subject: [MW:14145] alignment tolerance

Dear All,
 
what is the maximum alignment tolerance as per ASME Sec VIII Div 1?
 
Thanx
 
PSP
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...