Thursday, April 19, 2012

Re: [MW:14129] Re: regarding- thickness range for LTCS piping material for WPS

As per ASME Sec.IX QW451.1 thickness of test coupon is 1.5mm to mm means the thickness qualified limit is 1.5mm (Minimum) and 2T(Maximum).
In your case, If you use 7.11mm thickness specimen for PQR then the Thickness Qualified limit will be 1.5mm to 14.22mm.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: Raghuram Bathula <raghurambathula@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, April 19, 2012 3:09 PM
Subject: [MW:14128] Re: regarding- thickness range for LTCS piping material for WPS

what is your design code?
As per ASME it will be T-2T, however for piping (B31.3) this range can
be used if PTC's are provided for the thickness ranges as specified in
Table 323.3.1, else it will be T to T+6mm

Best regards

On Apr 19, 10:42 am, Darshan Maheshwari <darshan.maheshw...@yahoo.com>
wrote:
> Can any body suggest what thickness range is applied for qualifying a WPS (for thickness 7.11mm) for LTCS piping material. Please provide reference also.
>
> Regards,
>
> Darshan Maheshwari.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.