Re: [MW:13673] Thickness Range Qualified by Welder - ASME Sec. IX

Dear friend,

As per below clause upto 12 mm 2t qualify, and for maximum take 13 and high thk plate with minimum 3 layers in single process.

Regards,
Shaunak,

On Feb 14, 2012 9:35 AM, "Vivek Jadhav (HFGR)" <VJadhav@ccc.ae> wrote:

Dear Experts,

Can someone explain me following ASME clause regarding thickness range qualified by welder & is it OK if a welder welds 13 mm & above with 3 or more layers, he is qualified for maximum thickness ( e.g. 50mm or more )

 

 

 

 

 

 

 

 

 

Best Regards,

Vivek Jadhav

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35536] RANGE ASME SEC IX

Dear All we have qualified WPS for ( ASME SEC IX) 1. BASE plate 8 mm ( 8TO 16 mm RANGE WITH IMPACT )  2 . BASE plate 25 mm ( 16TO 50mm RANGE...