Re: [MW:13654] ASTM A890 Gr 6A Casting Repair procedure

Hi,

Curious to know the application of these castings?

ASTM E165 (Liquid Penetration examination)and ASME Sec Viii Div 1 App 7 outlines the method and
acceptance criteria of discontinuities.

If discontinuity is unacceptable, weld repair shall be performed in accordance with applicable
ASTM, castings shall be PWHT'd for major repairs in accordance with supplementary requirement
S33.

ASME Sec ix and ASTM A488 shall be followed for welding procedure qualification of repairs,
please check client specification for impact requirements or tell us what is MDMT to decide
impact testing,Absorbed energy shall be 48J average and 36J single value minimum. after repair
welding hardness shall not exceed HRC 32 or HV 319.

Surface finish shall be White Pickled

Matched fillers with GTAW and shielding gas Ar + 2% Nitrogen are used for welding repairs if
PWHT is carried out.

Suggest to consult Filler supplier to achieve best results.


Regards
Manpreet Singh




On Fri, 10 Feb 2012 18:14:10 +0530 wrote
>Hi everybody,



I have been deputed for a Casting Repair upgradation.



Please suggest me Casting Repair procedure and How many PT rounded

indications shall I accept?



Material is ASTM A 890 Gr 6A SDSS



Appreciated for fast response.







Shanmuga Navaneethan

Sr.Welding Engineer



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...