Hello ALL,
Can anybody suggest me suitable filler of ER series for welding Kanthal APM bar to SS 316 plate.
Regards
S G Dixit
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...