Hi

A welder can basically qualified on a qualified WPS. In your case, the WPS is with backing but the welder is qualified without backing which is conflicting. Even though the  deletion of backing is not an essential variable for a WPS, either you have to rewrite the WPS with backing (if qualified for that) or have to qualify the welder on without backing WPS. In addition, the WPS number shall be reflected in the welder qualification certificate.

See the excerpt below from Sec IX which clearly states the performance qualification on qualified WPS

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Aly
Sent: Tuesday, January 31, 2012 8:07 PM
To: materials-welding@googlegroups.com
Subject: [MW:13596] WPS with baking for welding single side welded Joint without backing with qualified Welder without backing

 

Dear experts,

 

Could you please clarify following;

 

If I have qualified WPS with backing & qualified Welder without backing; with this can we weld single side welded joint without backing.Please reply me in the light of ASME SEC IX.

 

Thanks in advance

 

Ali Mhaskar

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone