Tuesday, January 10, 2012

Re: [MW:13446] NDE FOR BUTT WELD

Dear Sir,
            As per your first photo only UT is possible since space constraint for the film.

On Tue, Jan 10, 2012 at 4:38 PM, balaganapathy lingam r <balashivasa@gmail.com> wrote:
Dear Sir,
             Both are possible but we have to slightly bend the film(cassette) to get a clear image(i.e) :- the cassette must be very closely packed with the joint. I think this will be giving you a good result. 

On Tue, Jan 10, 2012 at 3:27 PM, Desai Jignesh (Mumbai - Piping) <J.J.Desai@ticb.com> wrote:

Can somebody write me about the possibility of either radiography OR Ultrasonic testing of attached butt weld?

 

We have tried to carry out radiography with and without non metallic support as in the attached snaps but image is not clear.

 

Regds/Jignesh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
R.Balaganapathylingam
 
QC - Lead Engineer,
FLSmidth.




--
R.Balaganapathylingam
 
QC - Lead Engineer,
FLSmidth.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...