______________________________________________________________________________________________________________________________________
From: Wolfgang.Schmitz@vdeh.de [mailto:Wolfgang.Schmitz@vdeh.de]
Sent: Monday, January 09, 2012 8:53 PM
To: Bathula Raghuram (Mumbai - PIPING)
Cc: Stefanie.Brockmann@vdeh.de
Subject: Request to yield values for the steel grades TTStE 36 to SEW
089-70 and for steel grade TTSt 35 N to SEW 680-70, at 50 ° C. Dear Mr
Bathula,
We regret but the technical informations SEW 089 and SEW 680 contains
not yield stress information by 50 ° C. So we can not give you any
information.
Perhaps the following information will help you further.
TTStE 36 to SEW 089-70
<= 16 mm 36 kg/mm2 yield strength at room temperature +20 ° C.
TTSt 35 N to SEW 680-70(valid for longitudinal samples)
<= 10 mm wall thickness or diameter 23 kg/mm2 yield strength at room
temperature +20 ° C.
Yours sincerely
Steel Institute VDEh
European Steel Registration Office
i.A.
W. Schmitz
on behalf of Dr -Ing. H.-J. Wieland
Steel Institute VDEh
European Steel Registration Office
Sohnstraße 65
D-40237 Düsseldorf
Phone: +49/(0)211/6707-109
Fax: +49/(0)211/6707-421
E-mail: wolfgang.schmitz@wvstahl.de
Internet: http://www.vdeh.de bzw. www.stahl-online.de
Please visit our web-based material and steel database on www.stahldat.de
Disclaimer:
Messages sent by e-mail can be manipulated by third parties. For this
reason this e-mail is not legally binding.
On Dec 29 2011, 1:30 pm, "Bathula Raghuram (Mumbai - PIPING)"
<R.Bath...@ticb.com> wrote:
> We have very old shell and tube exchanger (30 years old) which has the following material. We need recheck with design calculation, however we are unable find the specification for these materials. Can anybody provide where can I get the allowable stresses and mechanical properties of this material, particularly we are looking for yield stress value of following material at 50 °C.
>
> I tried to contact German Iron and Steel Institute (VDEh) @ Heinz-Friedrich.H...@vdeh.de<mailto:Heinz-Friedrich.H...@vdeh.de>, but no response (http://www.stahl-online.de/english/Stahlinstitut_VDEh/Standards.php?h...)
> Plate material - TT st E36 SEW 089 (Google search ~ nearest equivalent SA 537 cl 1)
> Pipe material - TT st 35N SEW 680 (Google search ~ nearest equivalent SA 333 Gr 1/6)
>
> Filtered by Hosted Filtering
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment