complete line was pressurized for 24 hrs to see any leakage coming out
to soil top, but the line was also hydrotested spool basis before
backfill
Regards,
Srinivas
On 1/5/12, mohd.qce <mohd52100@gmail.com> wrote:
> Dear experts,
>
> Can any one give good and efficient method of underground(buried) pipe
> line leak testing method during hydrotest?
>
> Pipe: API 5L Gr 52 MS PSL-2.
> Length : Two section 50km+50km (2500 joints approx each section).
> Test pressure : 73.25 bar.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
Ohm Guru Namasivaya
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment