Thursday, January 5, 2012

[MW:13415] Filler welding for A351 Gr CD4 M Cu

Good morning,

I chose type E308 & E 308 L filler welding for A351 Gr CD4 M Cu
material, the choice was made, as per ASME Section II Part C code,

Question: Is it a good choice?

Thanks.

Best regards.
BENADJAL Redouane
Project engineer (SONATRACH Algeria)
E-mail: refazosaris@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...