We need to Weld repair the flare cone. Intially it was thought it is
SS 310, but after PMI it was found that it is 321. It was understood
that SS 321 was welded with E 310. Is it accepble to weld SS 321
with E 310 electrode. What are the pro and cons.
SS 321 and 310 are meant for high temp. applications. Please
eloborate the differences between them on application point of view.
Regards
Venkat
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments: