Silica means the sand,.due to blasting,size of the sand would become very minute and it will cause silicosys (lung desease) to the human who is breathing the same..
 
So internationaly sand blasting has been banned...
 
However copper slag can be used for abrasive blasting..  
 
 
 
 
-------Original Message-------
 
Date: 9/22/2010 6:52:13 PM
Subject: [MW:7145] Copper Slag Abrasive
 
Hi everyone,
                    I came across many coating specs which are having one common sentence " Silica sand and copper slag shall not be used for blasting".

What is the issue with using copper slag ? What are the dis advantages of copper slag?

--
- Sreejith Nair-

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

1 comment:

disha said...

Nice articles and your information valuable and good articles thank for the sharing information COPPER SLAG BLASTING

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...